Chapter 16: Cast Irons
-
Published:2007
Abstract
This chapter discusses the composition, properties, microstructure, grain formation, and fracture behavior of gray, white, ductile, and malleable cast iron and how these critical factors are affected when iron is heated to different temperatures prior to or during solidification.
You do not currently have access to this chapter.
Citation
Cast Irons, Steel Metallurgy for the Non-Metallurgist, By John D. Verhoeven, ASM International, 2007, p 175–188, https://doi.org/10.31399/asm.tb.smnm.t52140175
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Origin of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Solidification Structures of Steels and Cast Irons
Metallography and Microstructures
Trace (Minor) Elements in Cast Irons
Cast Iron Science and Technology
Alteration of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Computational Models for Prediction of Solidification Microstructure
Cast Iron Science and Technology
Principles of Thermal Analysis
Cast Iron Science and Technology
Phases and Microstructure of Superalloys
Superalloys Alloying and Performance
Volumetric Changes during the Solidification of Cast Iron
Cast Iron Science and Technology
Mechanical Properties of Gray Irons
Cast Iron Science and Technology
The Liquid State and Principles of Solidification of Cast Iron
Cast Iron Science and Technology