Abstract
Most quenched steels are tempered because the toughness of as-quenched steels is generally very poor. The tempering operation sacrifices strength for improvements in ductility and toughness. This chapter discusses the tempering process, the challenge of tempered martensite embrittlement, and the effect of wt% carbon on toughness. It also explains how alloying elements improve the hardenability and tempering response of plain carbon steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Tempering, Steel Metallurgy for the Non-Metallurgist, By John D. Verhoeven, ASM International, 2007, p 99–106, https://doi.org/10.31399/asm.tb.smnm.t52140099
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Steel Products and Properties
Metallurgy for the Non-Metallurgist (Second Edition)
Heat Treating of Alloy Steels
Practical Heat Treating (Second Edition)
Iron and Steel
Elementary Materials Science
Water-Hardening Tool Steels
Tool Steels (Fifth Edition)
Air-Hardening, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Heat Treatment of Malleable and Compacted-Graphite Irons
Heat Treating of Irons and Steels
295.0 Al-Cu-Si Heat-Treatable Sand Casting Alloy
Properties and Selection of Aluminum Alloys
Tempering of Steels
Steel Heat Treating Fundamentals and Processes
High-Carbon, High-Chromium, Cold-Work Tool Steels
Tool Steels (Fifth Edition)
Metallurgy of Steels and Related Boiler Tube Materials
Failure Investigation of Boiler Tubes A Comprehensive Approach