Failure Investigation of Boiler Tubes: A Comprehensive Approach
ASM International
ISBN electronic:
978-1-62708-253-2
Publication date:
2018
Book Chapter
Chapter 6.7: Operation-Related Failures
-
Published:2018
Abstract
This chapter examines boiler tube failures attributed to operation-related causes. It discusses failures due to rapid start-ups, excessive load swing, excessive heat inputs, poor water chemistry control, and water-treatment methods.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Operation-Related Failures, Failure Investigation of Boiler Tubes: A Comprehensive Approach, By Paresh Haribhakti, P.B. Joshi, Rajendra Kumar, ASM International, 2018, p 343–351, https://doi.org/10.31399/asm.tb.fibtca.t52430343
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Remaining Life Assessment of Boiler Tubes
Failure Investigation of Boiler Tubes A Comprehensive Approach
Acidic Pitting in Waterwall Tubing
Handbook of Case Histories in Failure Analysis
Materials for Boiler Tubes
Failure Investigation of Boiler Tubes A Comprehensive Approach
Uniform Corrosion of Carbon Steel Boiler Feedwater Tubes
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Rupture of a Carbon Steel Tube Because of Hydrogen-Induced Cracking and Decarburization
ASM Failure Analysis Case Histories: Power Generating Equipment
Hydrogen Damage of Waterwall Tubes
Handbook of Case Histories in Failure Analysis
Life Prediction for Boiler Components
Damage Mechanisms and Life Assessment of High-Temperature Components
Rupture of Low-Carbon Steel Boiler Tubes Because of Severe Overheating
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Corrosion-Fatigue Failure of Finned Stainless Steel Economizer Tubes Due to Differential Thermal Expansion
ASM Failure Analysis Case Histories: Pulp and Paper Processing Equipment
Cracking of Furnace Rings of Horizontal Multi-Tubular Boiler
ASM Failure Analysis Case Histories: Rail and Rolling Stock