Abstract
Combustion byproducts such as soot, ash, and abrasive particulates can inflict significant damage to boiler tubes through the cumulative effect of erosion. This chapter examines the types of erosion that occur on the fire side of boiler components and the associated causes. It discusses the erosive effect of blowing soot, steam, and fly ash as well as coal particle impingement and falling slag. It also includes several case studies.
You do not currently have access to this chapter.
Citation
Fire-Side Erosion, Failure Investigation of Boiler Tubes: A Comprehensive Approach, By Paresh Haribhakti, P.B. Joshi, Rajendra Kumar, ASM International, 2018, p 314–325, https://doi.org/10.31399/asm.tb.fibtca.t52430314
Download citation file:
Related Book Content
Introduction to Damage Mechanisms with Case Studies
Failure Investigation of Boiler Tubes A Comprehensive Approach
Remaining Life Assessment of Boiler Tubes
Failure Investigation of Boiler Tubes A Comprehensive Approach
Operation-Related Failures
Failure Investigation of Boiler Tubes A Comprehensive Approach
Acidic Pitting in Waterwall Tubing
Handbook of Case Histories in Failure Analysis
Rupture of a Carbon Steel Tube Because of Hydrogen-Induced Cracking and Decarburization
ASM Failure Analysis Case Histories: Power Generating Equipment
Uniform Corrosion of Carbon Steel Boiler Feedwater Tubes
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Materials for Boiler Tubes
Failure Investigation of Boiler Tubes A Comprehensive Approach
Rupture of Water Wall Tubes of a Boiler
ASM Failure Analysis Case Histories: Power Generating Equipment
Local Perforation of Boiler Tubes
ASM Failure Analysis Case Histories: Power Generating Equipment
Examination of Corroded Boiler Tubes
ASM Failure Analysis Case Histories: Power Generating Equipment