Abstract
This chapter provides an outline of the failure modes and mechanisms associated with most boiler tube failures in coal-fired power plants. Primary categories include stress rupture failures, water-side corrosion, fire-side corrosion, fire-side erosion, fatigue, operation failures, and insufficient quality control.
You do not currently have access to this chapter.
Citation
Introduction to Damage Mechanisms with Case Studies, Failure Investigation of Boiler Tubes: A Comprehensive Approach, By Paresh Haribhakti, P.B. Joshi, Rajendra Kumar, ASM International, 2018, p 147–149, https://doi.org/10.31399/asm.tb.fibtca.t52430147
Download citation file:
Related Book Content
Failures of Boilers and Related Equipment
Failure Analysis and Prevention
Fire-Side Erosion
Failure Investigation of Boiler Tubes A Comprehensive Approach
Fire-Side Corrosion
Failure Investigation of Boiler Tubes A Comprehensive Approach
Damage Mechanisms References
Failure Investigation of Boiler Tubes A Comprehensive Approach
Failures Due to Lack of Quality Control or Improper Quality Control
Failure Investigation of Boiler Tubes A Comprehensive Approach
Fatigue
Failure Investigation of Boiler Tubes A Comprehensive Approach
Water-Side Corrosion Failures
Failure Investigation of Boiler Tubes A Comprehensive Approach
Role of Water Chemistry in Boiler Tube Failure
Failure Investigation of Boiler Tubes A Comprehensive Approach
Failure of Boilers and Related Equipment
Analysis and Prevention of Component and Equipment Failures
Remaining Life Assessment of Boiler Tubes
Failure Investigation of Boiler Tubes A Comprehensive Approach