Elements of Metallurgy and Engineering Alloys
Chapter 30: Superalloys
-
Published:2008
Abstract
Superalloys are nickel, iron-nickel, and cobalt-base alloys designed for high-temperature applications, generally above 540 deg C. This chapter covers the metallurgy, composition, and properties of cast and wrought superalloys. It provides information on melting, heat treating, and secondary fabrication processes. It also covers coating technology, including aluminide diffusion and overlay coatings, and addresses the advantages and disadvantages of superalloys in various applications.
Sign in
ASM members
Member Sign InSuperalloys, Elements of Metallurgy and Engineering Alloys, Edited By F.C. Campbell, ASM International, 2008, p 563–581, https://doi.org/10.31399/asm.tb.emea.t52240563