Abstract
Aluminum has many outstanding properties, leading it to be used for a wide range of applications. It offers excellent strength-to-weight ratio, good corrosion and oxidation resistance, high electrical and thermal conductivity, exceptional formability, and relatively low cost. This chapter examines the metallurgy, composition, processing, and mechanical properties of aluminum and its alloys, both cast and wrought forms. It also covers heat treating and basic temper designations, including annealed, work hardened, solution heat treated, and solution heated treated and aged. The chapter concludes with information on corrosion and oxidation resistance.
Aluminum, Elements of Metallurgy and Engineering Alloys, Edited By F.C. Campbell, ASM International, 2008, p 487–508, https://doi.org/10.31399/asm.tb.emea.t52240487
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.