CAD Navigation Principles
-
Published:2019
Abstract
Over the revolutionary era of semiconductor technology, Computer-Aided Design Navigation (CADNav) tools have played an increasingly critical role in silicon debug and failure analysis (FA) in efforts to improve manufacturing yield while reducing time-to-market for integrated circuit (IC) products. This article encompasses the key principles of CADNav for various aspects of semiconductor FA and its importance for improved yield and profitability. An overview of the required input data and formats are described for both IC and package devices, along with key considerations and best practices recommended for fast fault localization, accurate root cause analysis, FA equipment utilization, efficient cross-team...
Sign in
ASM members
Member Sign InArpan Bhattacherjee, Martin Parley, CAD Navigation Principles, Microelectronics Failure Analysis: Desk Reference, 7th ed., Edited By Tejinder Gandhi, ASM International, 2019, p 262–268, https://doi.org/10.31399/asm.tb.mfadr7.t91110262
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!