Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
Abstract
This article introduces the wafer-level fault localization failure analysis (FA) process flow for an accelerated yield ramp-up of integrated circuits. It discusses the primary design considerations of a fault localization system with an emphasis on complex tester-based applications. The article presents examples that demonstrate the benefits of the enhanced wafer-level FA process. It also introduces the setup of the wafer-level fault localization system. The application of the wafer-level FA process on a 22 nm technology device failing memory test is studied and some common design limitations and their implications are discussed. The article presents a case study and finally...
Sign in
ASM members
Member Sign InS.H. Goh, Y.H. Chan, B.L. Yeoh, H. Hao, M.H. Thor, Z. Lin, C.M. Chua, S.H. Tan, L.S. Koh, W.P. Chua, Overview of Wafer-level Electrical Failure Analysis Process for Accelerated Yield Engineering, Microelectronics Failure Analysis: Desk Reference, 7th ed., Edited By Tejinder Gandhi, ASM International, 2019, p 1–9, https://doi.org/10.31399/asm.tb.mfadr7.t91110001
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!