The melting furnace is a critically important piece of equipment in a foundry; it influences the balance between the metal required by molding machines and the melting capacity. This chapter presents the features, types, advantages, and applications of furnaces suitable for iron and steels such as cupolas, induction furnaces, and arc furnaces.