Chapter 1: Basic Understanding of Gears
-
Published:1985
Abstract
This chapter presents the purpose, design, and function of a gear. It also presents the basic stresses applied to a gear tooth. The chapter provides an overview on the bending strength and characteristics of the gear tooth.
You do not currently have access to this chapter.
Citation
Basic Understanding of Gears, Systematic Analysis of Gear Failures, By Lester E. Alban, ASM International, 1985, p 1–25, https://doi.org/10.31399/asm.tb.sagf.t63420001
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Rolling-Contact Wear
Friction, Lubrication, and Wear Technology
Selection of Heat Treat Process for Optimum Gear Design
Heat Treatment of Gears A Practical Guide for Engineers
Fatigue and Life Prediction
Gear Materials, Properties, and Manufacture
Powder Metallurgy Gears
Powder Metallurgy
Basic Understanding of Gears
Gear Materials, Properties, and Manufacture
Friction, Lubrication, and Wear of Gears and Wind-Turbine Components
Friction, Lubrication, and Wear Technology