Abstract
Parts of machines and equipment that have previously been designed as wrought or fabricated parts, or as cast parts of metals other than steel, are often reconsidered as steel castings. This chapter presents bending test data for several junction designs of L and box sections and discusses redesign from fabrication, forgings, and cast iron. The chapter also includes the benefits of redesign.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Redesign As Steel Castings, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 10-1–10-13, https://doi.org/10.31399/asm.tb.sch6.t68200144
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Fatigue Failure of Titanium Alloy Compressor Blades
Handbook of Case Histories in Failure Analysis
Introduction to Steel Castings
Steel Castings Handbook (Sixth Edition)
Industrial Applications of Steel Castings
Steel Castings Handbook (Sixth Edition)
Purchasing Policy
Steel Castings Handbook (Sixth Edition)
Casting Alloys
Stainless Steels for Design Engineers
Advantages of Steel Castings
Steel Castings Handbook (Sixth Edition)
Quality Control and Quality Assurance
Steel Castings Handbook (Sixth Edition)
Cast-Weld Construction
Steel Castings Handbook (Sixth Edition)
Finishing, Heat Treatment and Inspection
Steel Castings Handbook (Sixth Edition)
Process Capability and Tolerances
Steel Castings Handbook (Sixth Edition)