Abstract
This chapter discusses the role of standards and specifications for steel castings. It defines specifications and discusses how certification, testing, examination, methods, practices, procedures, compositions, properties, facilities, statistical process control, and documentation relate to codes and standards. The chapter describes processes involved in the selection of specifications for steel castings. Further, it provides information on the cost of specifications.