Steel Castings Handbook (Sixth Edition)
Chapter 2: Industrial Applications of Steel Castings
-
Published:1995
Abstract
Steel castings are produced in thousands of designs for different applications. They fill needs in many industries, including transportation, construction machinery, earthmoving equipment, rolling mills, mining, oil and gas exploration, and power generation. This chapter touches upon the variety of applications for which steel castings can be supplied and the ranges of casting size and complexity. Photographs in this chapter provide an understanding of these applications, their size and complexity, and the types of cast steels produced.
Sign in
ASM members
Member Sign InIndustrial Applications of Steel Castings, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 2-1–2-40, https://doi.org/10.31399/asm.tb.sch6.t68200007
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!