Chapter 9: Thermodynamics of Microstructure Change
-
Published:2008
Abstract
This chapter provides a classification of the types of microstructural changes and transformations and then reviews each type. It presents the Johnson-Mehl-Avrami-Kolmogorov (JMAK) equation and explains the thermodynamics of eutectic solidification and eutectoid transformation. An appendix covers growth of eutectoid structure in carburized pearlite.
Thermodynamics of Microstructure Change, Thermodynamics of Microstructures, By Taiji Nishizawa, ASM International, 2008, p 259–285, https://doi.org/10.31399/asm.tb.tm.t52320259