Iron and Steel Castings Engineering Guide
Chapter 6: Engineering for Manufacturability and Integrity
-
Published:2022
Abstract
The casting engineer contributes to a successful component design by offering expertise in molding, core making, and material characteristics and by recommending the most suitable casting process to use to meet quality and cost targets. The casting engineer's responsibilities include recommending locator positioning; advising about lugs, hooks, or holes for casting handling through all processes; determining the choice of a parting plane and pouring orientation; designing cores for accurate positioning, suitable venting, and proper cleaning; guiding decisions about wall thicknesses and junctions; making suggestions about casting design to eliminate distortion; optimizing the gating design for slag-free metal; and establishing...
Sign in
ASM members
Member Sign InEngineering for Manufacturability and Integrity, Iron and Steel Castings Engineering Guide, By Jagan Nath, ASM International, 2022, p 63–102, https://doi.org/10.31399/asm.tb.isceg.t59320063
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!