Chapter 1: Casting Performance and Cost Drivers
-
Published:2022
Abstract
Engineered geometry and its microstructures impact casting performance. This chapter describes three interdependent disciplines that are needed to achieve product performance and cost targets, namely engineered geometry; target microstructure and chemistry; and optimum process for high integrity.
Topics
Microstructure,
Casting defects,
Cast iron,
Steel,
Automobiles and trucks,
Corrosion-resistant alloys,
Casting,
Austempering,
Alloy composition,
Castability,
Fatigue properties,
Impact toughness,
Wear resistance,
Brinell hardness,
Flow,
Tensile properties,
Materials selection,
Quality assurance and testing,
Casting equipment,
Phase constituents,
Solidification
You do not currently have access to this chapter.
Citation
Casting Performance and Cost Drivers, Iron and Steel Castings Engineering Guide, By Jagan Nath, ASM International, 2022, p 1–2, https://doi.org/10.31399/asm.tb.isceg.t59320001
Download citation file:
Related Book Content
Aluminum Casting Applications
Aluminum Castings Engineering Guide
Casting Alloys
Stainless Steels for Design Engineers
Process Selection Guidelines
Aluminum Castings Engineering Guide
Casting
Metals Fabrication Understanding the Basics
Castings
Titanium: A Technical Guide (Second Edition)
Billet Casting Principles and Practice
Aluminum Extrusion Technology
Casting, Forming, and Forging
Gear Materials, Properties, and Manufacture
Introduction
Aluminum Alloy Castings Properties, Processes, and Applications