Chapter 11: Two New Classes of Stainless Steel
-
Published:2010
Abstract
This chapter provides a detailed discussion on microstructure, properties, and applications of two classes of stainless steel: duplex stainless steel and precipitation-hardening steel.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Two New Classes of Stainless Steel, The History of Stainless Steel, By Harold M. Cobb, ASM International, 2010, p 185–192, https://doi.org/10.31399/asm.tb.hss.t52790185
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Stainless Steels
Metallography of Steels Interpretation of Structure and the Effects of Processing
Pump Shaft Failure
ASM Failure Analysis Case Histories: Design Flaws
Compositions
Stainless Steels for Design Engineers
Alloy Classification and Compositions
Powder Metallurgy
Introduction to the Selection of Stainless Steels
Welding, Brazing, and Soldering
Corrosion of Duplex Stainless Steel Weldments
Corrosion of Weldments
Material Issues in the Pharmaceutical Industry
Corrosion: Environments and Industries
Heat Treating of Austenitic and Duplex Stainless Steels
Heat Treating of Irons and Steels
Stainless Steels
Metallurgy for the Non-Metallurgist (Second Edition)
Stainless Steels
Alloying Understanding the Basics