This appendix lists the readings of specified hardness limits for H-steels, along with graphs showing the distance from the quenched surface against hardness values.
Topics
Dislocations,
Crystal morphology,
Grain morphology,
Microstructure,
Carbon steel,
Low-alloy steel,
Structural steel,
Hardenability testing,
Precipitation hardening,
Annealing,
Austenitizing,
Normalizing,
Oil quenching,
Water quenching,
Austempering,
Martempering,
Tempering,
Chemical composition,
Rate of decomposition,
Hardenability,
Fracture toughness,
Hardness,
Plastic deformation properties,
Tensile properties,
Heat transfer properties,
Recrystallization temperature,
Phase,
Phase transformations,
Steel,
Quenching
You do not currently have access to this chapter.
Citation
Hardenability Bands for H-Steels, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 441–468, https://doi.org/10.31399/asm.tb.phtpclas.t64560441
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Heat Treating of Carbon Steels
Practical Heat Treating (Second Edition)
Calculation of Hardenability in High-Carbon Steels
Steel Heat Treating Fundamentals and Processes
Quench Process Sensors
Steel Heat Treating Fundamentals and Processes
Quenching
Practical Induction Heat Treating (Second Edition)
Fluidized-Bed Quenching
Steel Heat Treating Fundamentals and Processes
Quench Sensitivity of Aluminum Alloys
Heat Treating of Nonferrous Alloys
Cracks in Flame Hardened Operation Handles
ASM Failure Analysis Case Histories: Processing Errors and Defects
Spray Quenching
Steel Heat Treating Fundamentals and Processes
Induction Hardening Gears
Heat Treatment of Gears A Practical Guide for Engineers
Quenching with Molten Metal
Steel Heat Treating Technologies