Appendix 8: Compositions of Standard Carbon H-Steels and Standard Carbon Boron H-Steels
-
Published:1996
Abstract
This appendix contains tables listing the chemical compositions of standard carbon H-steels and standard carbon boron H-steels and the hardenability characteristics of alloys.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Compositions of Standard Carbon H-Steels and Standard Carbon Boron H-Steels, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 413–414, https://doi.org/10.31399/asm.tb.phtpclas.t64560413
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Classification of Carbon and Low-Alloy Steels
Practical Heat Treating Basic Principles
Hardenability Calculation of Carbon and Low-Alloy Steels with Low or Medium Carbon
Steel Heat Treating Fundamentals and Processes
Heat Treating of Carbon Steels
Heat Treating of Irons and Steels
Hardenability and Heat Treatment
Steel Castings Handbook (Sixth Edition)
Heat Treatment of Carbon and Low-Alloy Steels
Practical Heat Treating Basic Principles
Introduction to Gear Heat Treatment
Heat Treatment of Gears A Practical Guide for Engineers
Compositions of Standard Carbon Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Carbon and Alloy Steels
Alloying Understanding the Basics
Steel Cross Reference
Heat Treating of Irons and Steels
Stress-Corrosion Cracking of Carbon and Low-Alloy Steels (Yield Strengths Less Than 1241 MPa)
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)