Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Chapter 10: Illustrative Examples
-
Published:1996
Abstract
This chapter contains problems that illustrate the calculation or determination of such items as ideal critical diameter, the Jominy curve, and the severity of quench by methods. It presents solutions for the calculation of the effect of prior austenite grain size, carbon content, chromium content, and molybdenum content on ideal critical diameter. The chapter also contains solutions for calculation of Jominy curves and determination of minimum hardness of quenched steels, tempered hardness, ideal critical diameter, severity of quench, heat treatment, and effect of tempering during heat-up to tempering temperature.
Illustrative Examples, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 365–387, https://doi.org/10.31399/asm.tb.phtpclas.t64560365
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!