Tensile Testing (Second Edition)
Edited by
ASM International
ISBN electronic:
978-1-62708-355-3
Publication date:
2004
Search within book:
Abstract
This chapter contains tables listing room-temperature tensile yield strength comparisons of metals and plastics and room-temperature tensile modulus of elasticity comparisons of various materials.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Reference Tables, Tensile Testing, 2nd ed., Edited By J.R. Davis, ASM International, 2004, p 273–277, https://doi.org/10.31399/asm.tb.tt2.t51060273
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Glossary of Terms: Mechanical Testing and Evaluation
Mechanical Testing and Evaluation
Aluminum Structural Design
Properties and Selection of Aluminum Alloys
Etchants for Revealing Macrostructure
Metallography Principles and Practice
Attack Polishing Procedures
Metallography Principles and Practice
Chemical Polishing Solutions
Metallography Principles and Practice
Description of Hardness Code and Specification of Hardness Numbers for Metals
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Corrosion Rate Conversion
Corrosion: Environments and Industries
Corrosion Rate Conversion
Corrosion: Fundamentals, Testing, and Protection
Electrolytic Polishing Solutions
Metallography Principles and Practice
Dislocation Etching Techniques
Metallography Principles and Practice