Tensile Testing (Second Edition)
Chapter 4: Tensile Testing Equipment and Strain Sensors
-
Published:2004
Abstract
This chapter reviews the current technology and examines force application systems, force measurement, strain measurement, important instrument considerations, gripping of test specimens, test diagnostics, and the use of computers for gathering and reducing data. The influence of the machine stiffness on the test results is also described, along with a general assessment of test accuracy, precision, and repeatability of modern equipment. The chapter discusses various types of testing machines and their operations. Emphasis is placed on strain-sensing equipment. The chapter briefly describes load condition factors, such as strain rate, machine rigidity, and various testing modes by load control, speed...
Sign in
ASM members
Member Sign InTensile Testing Equipment and Strain Sensors, Tensile Testing, 2nd ed., Edited By J.R. Davis, ASM International, 2004, p 65–89, https://doi.org/10.31399/asm.tb.tt2.t51060065
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.