Surface cleanliness requirements depend on which nitrocarburizing process is selected for component treatment. This chapter discusses the processes involved in some of the more commonly used precleaning methods for gas ferritic nitrocarburizing and provides information on the methods used to accomplish enhanced plasma cleaning.