Chapter 14: Processing with Nitriding
-
Published:2003
Abstract
The nitriding process can be applied to various materials and part geometries. This chapter focuses on tool steels, pure irons, low-alloy steels, and maraging steels. Various considerations such as the surface metallurgy requirements of the die, including case depth, compound layer formation, and temperature, are also discussed in this chapter. The chapter also addresses steel selection and surface metallurgy of gears.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Processing with Nitriding, Practical Nitriding and Ferritic Nitrocarburizing, By David Pye, ASM International, 2003, p 153–161, https://doi.org/10.31399/asm.tb.pnfn.t65900153
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Selection of Materials for Deep-Drawing Dies
Metalworking: Sheet Forming
Fluidized-Bed Heat Treating Equipment
Steel Heat Treating Technologies
Heat Treatment of Steel Gears
Heat Treating of Irons and Steels
Use of Test Coupons for Process Verification
Practical Heat Treating (Second Edition)
Classification and Selection of Tool Steels
Tool Steels (Fifth Edition)
Tribology of Nitrided and Nitrocarburized Steels
Friction, Lubrication, and Wear Technology
Introduction
Tool Steels (Fifth Edition)
Failure Analysis in Tool Steels
Failure Analysis of Heat Treated Steel Components
Tool Steels
Alloying Understanding the Basics
An Introduction to Nitriding
Practical Nitriding and Ferritic Nitrocarburizing