Practical Nitriding and Ferritic Nitrocarburizing
Chapter 6: Salt Bath Nitriding
-
Published:2003
Abstract
This chapter presents the salts used and the process advantages of salt bath nitriding. It describes bath testing and analysis including the materials and equipment, analysis procedure, and determination of sodium carbonate and sodium cyanate for titration testing of the nitriding salt bath. The chapter explains the procedures for maintenance of the salt bath and related equipment. It also discusses safety precautions and design parameters for furnace equipment.
Sign in
ASM members
Member Sign InSalt Bath Nitriding, Practical Nitriding and Ferritic Nitrocarburizing, By David Pye, ASM International, 2003, p 53–63, https://doi.org/10.31399/asm.tb.pnfn.t65900053