Practical Nitriding and Ferritic Nitrocarburizing
Chapter 5: Furnace Equipment and Control Systems
-
Published:2003
Abstract
This chapter provides a discussion of nitriding furnace equipment and control systems. The discussion covers the essential design criteria of the furnace, types of nitriding furnaces, insulation for the reduction of furnace heat losses, and factors influencing furnace configuration and design. It also covers the processes involved in the construction and maintenance of retorts, methods for sealing a retort to prevent ammonia leaks, and safety precautions to be taken while using ammonia. Further, the chapter provides information on the factors for choosing a heating medium and discusses the processes involved in controlling temperature, gas dissociation, oxygen probes, and nitriding...
Sign in
ASM members
Member Sign InFurnace Equipment and Control Systems, Practical Nitriding and Ferritic Nitrocarburizing, By David Pye, ASM International, 2003, p 39–52, https://doi.org/10.31399/asm.tb.pnfn.t65900039
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.