Chapter 3: How Does the Nitriding Process Work?
-
Published:2003
Abstract
Several process parameters must be considered to ensure success in achieving desired metallurgical properties and to minimize distortion. This chapter provides a detailed discussion on the liberation of nitrogen, dissociation of the gas at the selected nitriding temperature, why ammonia is used, distortion, and preheat treatment.
Topics
Nitriding
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
How Does the Nitriding Process Work?, Practical Nitriding and Ferritic Nitrocarburizing, By David Pye, ASM International, 2003, p 23–29, https://doi.org/10.31399/asm.tb.pnfn.t65900023
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Distortion
Practical Nitriding and Ferritic Nitrocarburizing
Furnace Equipment and Control Systems
Practical Nitriding and Ferritic Nitrocarburizing
Why Nitride?
Practical Nitriding and Ferritic Nitrocarburizing
Nitriding in Fluidized Beds
Practical Nitriding and Ferritic Nitrocarburizing
Residual Stresses and Distortion in Thermochemically Treated Steels
Steel Heat Treating Technologies
Nitridation
High-Temperature Corrosion and Materials Applications
Stress-Corrosion Cracking of Copper Absorber Tubes in an Air-Conditioning Unit
ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure
Use of Ultrasonic Inspection to Detect Creep Rupture in Stainless Steel Headers of an Ammonia-Plant Reformer Furnace
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Investigation of Distribution Manifolds from the Cooling Unit of an Ammonia Synthesis Plant
ASM Failure Analysis Case Histories: Chemical Processing Equipment
An Introduction to Nitriding
Practical Nitriding and Ferritic Nitrocarburizing