Abstract
The unique advantages of the nitriding process were recognized by German researchers in the early 1920s. It was used to treat steels for applications that required: high torque, high wear resistance; abrasive wear resistance; corrosion resistance; and high surface compressive strength. This chapter focuses on key process considerations and factors that helped nitriding gain acceptance. These factors include a low-temperature process, no quench requirement, minimal distortion, high hardness values, and resistance to oxidation.
Topics
Dimensional distortion,
Cast iron,
Carbon steel,
Stainless steel,
Chromium steel,
Chromium-molybdenum steel,
Air-hardening cold work tool steel,
High-speed tool steel,
Hot work tool steel,
Indentation hardness testing,
Salt baths,
Fluidized-bed furnaces,
Bell-type furnaces,
Retort furnaces,
Salt bath furnaces,
Vacuum furnaces,
Nitriding,
Nitrocarburizing,
Case hardening,
Materials selection,
Oxidation resistance,
Hardness
You do not currently have access to this chapter.
Citation
Why Nitride?, Practical Nitriding and Ferritic Nitrocarburizing, By David Pye, ASM International, 2003, p 13–22, https://doi.org/10.31399/asm.tb.pnfn.t65900013
Download citation file:
Related Book Content
Distortion
Practical Nitriding and Ferritic Nitrocarburizing
How Does the Nitriding Process Work?
Practical Nitriding and Ferritic Nitrocarburizing
Residual Stresses and Distortion in Thermochemically Treated Steels
Steel Heat Treating Technologies
An Introduction to Nitriding
Practical Nitriding and Ferritic Nitrocarburizing
Control of the Compound Zone or White Layer
Practical Nitriding and Ferritic Nitrocarburizing
Residual Stresses, Distortion, and Heat Treatment
Steels: Processing, Structure, and Performance (Second Edition)
Analysis of Distortion and Deformation
Failure Analysis and Prevention (2021 Edition)
Processing with Nitriding
Practical Nitriding and Ferritic Nitrocarburizing
Press Quenching
Steel Heat Treating Fundamentals and Processes