Principles of Brazing
Chapter 1: Introduction
-
Published:2005
Abstract
Brazing and soldering jointly represent one of several methods for joining solid materials. This chapter summarizes the principal characteristics of the various joining methods. It then discusses key parameters of brazing including surface energy and tension, wetting and contact angle, fluid flow, filler spreading characteristics, surface roughness of components, dissolution of parent materials, new phase formations, significance of the joint gap, and the strength of metals. The chapter also describes issues in processing aspects that must be considered when designing a joint, and the health, safety, and environmental aspects of brazing.
Sign in
ASM members
Member Sign InIntroduction, Principles of Brazing, By David M. Jacobson, Giles Humpston, ASM International, 2005, p 1–46, https://doi.org/10.31399/asm.tb.pb.t51230001
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.