Optical Microscopy of Fiber-Reinforced Composites
Chapter 15: The Effects of Lightning Strikes on Polymeric Composites
-
Published:2010
Abstract
Lightning damage in polymer composites, as in metal structures, is manifested by damage at both the macroscopic or visual level and within the material microstructure. In addition to visual damage assessment, non-destructive inspection techniques are employed to detect damage within the composite part. This chapter describes the macroeffects of a lightning strike on composites and discusses the methods involved in the assessment of microstructural damage in composites.
Sign in
ASM members
Member Sign InThe Effects of Lightning Strikes on Polymeric Composites, Optical Microscopy of Fiber-Reinforced Composites, By Brian S. Hayes, Luther M. Gammon, ASM International, 2010, p 245–259, https://doi.org/10.31399/asm.tb.omfrc.t53030245
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.