Chapter 11: Impact Response of Composites
-
Published:2010
Abstract
As fiber-reinforced polymeric composites continue to be used in more damage-prone environments, it is necessary to understand the response of these materials when subjected to impact from foreign objects. This chapter provides an overview of the analysis methods for impact-damaged composites. It discusses the causes and effects of various failure mechanisms in composite materials. The failure mechanisms covered are brittle-matrix composite failure, tough-matrix composite failure, thermoplastic-matrix composite failure mechanisms, untoughened thermoset-matrix composite failure mechanisms, toughened thermoset-matrix composite failure mechanisms, particle interlayer-toughened composite failure mechanisms, and dispersed-phase, rubber-toughened thermoset-matrix composite failure mechanisms.
Sign in
ASM members
Member Sign InImpact Response of Composites, Optical Microscopy of Fiber-Reinforced Composites, By Brian S. Hayes, Luther M. Gammon, ASM International, 2010, p 193–210, https://doi.org/10.31399/asm.tb.omfrc.t53030193
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.