Gear Materials, Properties, and Manufacture
Chapter 10: Nitriding
-
Published:2005
Abstract
Nitriding is a surface hardening heat treatment that introduces nitrogen into the surface of steel while it is in the ferritic condition. Gas nitriding using ammonia as the nitrogen-carrying species is the most commonly employed process and is emphasized in this chapter. Nitriding produces a wear- and fatigue-resistant surface on gear teeth and is used in applications where gears are not subjected to high shock loads or contact stress. It is useful for gears that need to maintain their surface hardness at elevated temperatures. Gears used in industrial, automotive, and aerospace applications are commonly nitrided. This chapter discusses the...
Sign in
ASM members
Member Sign InNitriding, Gear Materials, Properties, and Manufacture, Edited By J.R. Davis, ASM International, 2005, p 227–244, https://doi.org/10.31399/asm.tb.gmpm.t51250227
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.