Skip Nav Destination
September 12–15, 2022
View ASM Events page>
ASM Technical Books
Gear Materials, Properties, and Manufacture
Edited by
ASM International
ISBN electronic:
978-1-62708-345-4
Publication date:
2005
Book Chapter
Chapter 6: Casting, Forming, and Forging
-
Published:2005
Abstract
Gear manufacture depends on machinery available, design specifications or requirements, cost of production, and type of material from which the gear is to be made. This chapter discusses the processes involved in methods for manufacturing gears, namely casting, forming, and forging.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Casting, Forming, and Forging, Gear Materials, Properties, and Manufacture, Edited By J.R. Davis, ASM International, 2005, p 129–137, https://doi.org/10.31399/asm.tb.gmpm.t51250129
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Forging and Forming
Superalloys: A Technical Guide (Second Edition)
Fabrication and Finishing of Metal Products
Metallurgy for the Non-Metallurgist (Second Edition)
Fabrication of Wrought Stainless Steels
Metals Handbook Desk Edition (2nd Edition)
Metalworking
Beryllium Chemistry and Processing
Titanium
Elements of Metallurgy and Engineering Alloys
Processing of Titanium and Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)
Forging of Discontinuously Reinforced Aluminum Composites
Metalworking: Bulk Forming
Principles of Forging Machines
Cold and Hot Forging Fundamentals and Applications
Forging of Aluminum Alloys
Metalworking: Bulk Forming