Chapter 10: Selection of Heat Treat Process for Optimum Gear Design
-
Published:2000
Abstract
The successful design and manufacture of gears are influenced largely by design requirements, material selection, and proper heat treatment. This chapter addresses the cost factors and tradeoffs involved in selecting a material, design features, and a heat treating process to optimize gear performance for a particular application.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Selection of Heat Treat Process for Optimum Gear Design, Heat Treatment of Gears: A Practical Guide for Engineers, By A.K. Rakhit, ASM International, 2000, p 185–188, https://doi.org/10.31399/asm.tb.htgpge.t67320185
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Rolling-Contact Wear
Friction, Lubrication, and Wear Technology
Selected References
Heat Treatment of Gears A Practical Guide for Engineers
Powder Metallurgy Gears
Powder Metallurgy
Heat Treatment of Gears
Heat Treatment of Gears A Practical Guide for Engineers
Selection of Wrought Precipitation-Hardening Stainless Steels
Welding, Brazing, and Soldering
Introduction to Metals Process Simulation
Metals Process Simulation
Induction Hardening of Gears and Gear-Like Components
Induction Heating and Heat Treatment
Corrosion of Wrought Stainless Steels
Metals Handbook Desk Edition (2nd Edition)
Why Tools and Dies Fail
Failure Analysis and Prevention
Magnetic Barkhausen Noise for Nondestructive Inspection of Gears
Nondestructive Evaluation of Materials