Heat Treatment of Gears: A Practical Guide for Engineers
Chapter 10: Selection of Heat Treat Process for Optimum Gear Design
-
Published:2000
Abstract
The successful design and manufacture of gears are influenced largely by design requirements, material selection, and proper heat treatment. This chapter addresses the cost factors and tradeoffs involved in selecting a material, design features, and a heat treating process to optimize gear performance for a particular application.
Sign in
ASM members
Member Sign InSelection of Heat Treat Process for Optimum Gear Design, Heat Treatment of Gears: A Practical Guide for Engineers, By A.K. Rakhit, ASM International, 2000, p 185–188, https://doi.org/10.31399/asm.tb.htgpge.t67320185
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.