Fatigue and Durability of Metals at High Temperatures
Chapter 6: Total Strain-Based Strain-Range Partitioning—Isothermal and Thermomechanical Fatigue
-
Published:2009
Abstract
This chapter explains why it is sometimes necessary to separate inelastic from elastic strains and how to do it using one of two methods. It first discusses the direct calculation of strain-range components from experimental data associated with large strains. It then explains how the method can be extended to the treatment of very low inelastic strains by adjusting tensile and compressive hold periods and continuous cycling frequencies. The chapter then begins the presentation of the second approach, called the total strain-range method, so named because it combines elastic and inelastic strain into a total strain range. The discussion...
Sign in
ASM members
Member Sign InTotal Strain-Based Strain-Range Partitioning—Isothermal and Thermomechanical Fatigue, Fatigue and Durability of Metals at High Temperatures, By S.S. Manson, G.R. Halford, ASM International, 2009, p 111–154, https://doi.org/10.31399/asm.tb.fdmht.t52060111
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!