Fatigue and Durability of Metals at High Temperatures
Chapter 2: Creep Rupture
-
Published:2009
Abstract
This chapter focuses on creep-rupture failure, or more precisely, the time required for such a failure to occur at a given stress and temperature. It begins with a review of creep-rupture phenomena and the various ways creep-rupture data are presented and analyzed. It then examines a large collection of creep-rupture data corresponding to different alloy designations and heat treatments, identifying key relationships, similarities, and differences. It also presents a test method developed by the authors in which twelve materials are tested over a range of temperature, stress, and time in order to determine multiheat constants that are then used...
Sign in
ASM members
Member Sign InCreep Rupture, Fatigue and Durability of Metals at High Temperatures, By S.S. Manson, G.R. Halford, ASM International, 2009, p 21–41, https://doi.org/10.31399/asm.tb.fdmht.t52060021
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!