Damage Mechanisms and Life Assessment of High-Temperature Components
Chapter 8: Materials for Advanced Steam Plants
-
Published:1989
Abstract
Increasing the efficiency of power plants by operating at higher temperatures and pressures and adding a double-reheat feature comes at the expense of shortened lifetimes for critical components. This chapter provides an overview of the material-related problems associated with advanced steam plants and their respective solutions. The discussion covers the selection of materials on a component-specific basis for boilers as well as steam turbines.