Chapter 7: Petroleum Reactor Pressure-Vessel Materials for Hydrogen Service
-
Published:1989
Abstract
This chapter covers the failure modes and mechanisms of concern in hydroprocessing reactor vessels and the methods used to assess lifetime and performance. It begins with a review of the materials used in the construction of pressure-vessel shells, the challenges they face, and the factors that determine shell integrity. The discussion addresses key properties and design parameters including allowable stress, fracture toughness, the effect of microstructure and composition on embrittlement, high-temperature creep, and subcritical crack growth. The chapter also provides information on the factors that affect cladding integrity and ends with a section on life-assessment techniques.
Sign in
ASM members
Member Sign InPetroleum Reactor Pressure-Vessel Materials for Hydrogen Service, Damage Mechanisms and Life Assessment of High-Temperature Components, By R. Viswanathan, ASM International, 1989, p 329–382, https://doi.org/10.31399/asm.tb.dmlahtc.t60490329
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.