Damage Mechanisms and Life Assessment of High-Temperature Components
Chapter 4: Fatigue
-
Published:1989
Abstract
This chapter describes the phenomenological aspects of fatigue and how to assess its effect on the life of components operating in high-temperature environments. It explains how fatigue is measured and expressed and how it is affected by loading conditions (stress cycles, amplitude, and frequency) and factors such as temperature, material defects, component geometry, and processing history. It provides a detailed overview of the damage mechanisms associated with high-cycle and low-cycle fatigue as well as thermal fatigue, creep-fatigue, and fatigue-crack growth. It also demonstrates the use of tools and techniques that have been developed to quantify fatigue-related damage and its...
Sign in
ASM members
Member Sign InFatigue, Damage Mechanisms and Life Assessment of High-Temperature Components, By R. Viswanathan, ASM International, 1989, p 111–182, https://doi.org/10.31399/asm.tb.dmlahtc.t60490111
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!