Damage Mechanisms and Life Assessment of High-Temperature Components
Chapter 1: Introduction and Overview
-
Published:1989
Abstract
The ability to accurately assess the remaining life of components is essential to the operation of plants and equipment, particularly those in service beyond their design life. This, in turn, requires a knowledge of material failure modes and a proficiency for predicting the near and long term effects of mechanical, chemical, and thermal stressors. This chapter presents a broad overview of the types of damage to which materials are exposed at high temperatures and the approaches used to estimate remaining service life. It explains how operating conditions in power plants and oil refineries can cause material-related problems such as...
Sign in
ASM members
Member Sign InIntroduction and Overview, Damage Mechanisms and Life Assessment of High-Temperature Components, By R. Viswanathan, ASM International, 1989, p 1–20, https://doi.org/10.31399/asm.tb.dmlahtc.t60490001
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.