Abstract
Induction heating has found widespread use as a method to raise the temperature of a metal prior to forming or joining, or to change its metallurgical structure. However, induction heating has specialized capabilities that make it suitable for applications outside of metal treatment and fabrication. This chapter summarizes some of the special applications of induction heating, including those in the plastics, packaging, electronics, glass, chemical, and metal-finishing industries. The chapter concludes with a discussion of the application of induction heating for vacuum processes.
Sign in
ASM members
Member Sign InSpecial Applications of Induction Heating, Elements of Induction Heating: Design, Control, and Applications, By S. Zinn, S. L. Semiatin, ASM International, 1988, p 281–313, https://doi.org/10.31399/asm.tb.eihdca.t65220281
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.