Elements of Induction Heating: Design, Control, and Applications
Chapter 8: Coil Design and Fabrication
-
Published:1988
Abstract
Coil design for induction heating has been developed and refined over time based on the theoretical principles applied in practice to several simple inductor geometries such as the classical solenoidal coil. This chapter reviews the fundamental considerations in the design of inductors and describes some of the most widely used coils and common design modifications. Specialty coil designs for specific applications are also discussed. The chapter concludes with sections devoted to coil fabrication and design of power-supply leads.
Sign in
ASM members
Member Sign InCoil Design and Fabrication, Elements of Induction Heating: Design, Control, and Applications, By S. Zinn, S. L. Semiatin, ASM International, 1988, p 185–240, https://doi.org/10.31399/asm.tb.eihdca.t65220185
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.