This data set contains the results of uniaxial tensile tests of a wide range of aluminum casting alloys conducted at high temperatures from 100 to 370 deg C, subzero temperatures from -269 to -28 deg C, and room temperature after holding at high temperatures from 100 to 370 deg C. In most cases, tests were made of several lots of material of each alloy and temper. The results for the several lots were then analyzed together graphically and statistically, and the averages were normalized to the room-temperature typical values. For some alloys, "representative" values (raw data) rather than typical...