Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications
Chapter 11: Tribology of Plastics and Elastomers
-
Published:2021
Abstract
This chapter covers the friction and wear behaviors of plastics and elastomers. It begins by describing the molecular differences between the two types of polymers and their typical uses. It then discusses the important attributes of engineering plastics and their suitability for applications involving friction, erosion, and adhesive and abrasive wear. It also discusses the tribology of elastomers and rubber along with their basic differences and the conditions under which they produce Schallamach waves. It includes information on polymer composites as well.
Sign in
ASM members
Member Sign InTribology of Plastics and Elastomers, Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications, By Kenneth G. Budinski, Steven T. Budinski, ASM International, 2021, p 301–334, https://doi.org/10.31399/asm.tb.tpsfwea.t59300301
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.