Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications
Chapter 10: Tribological Properties of Ceramics, Cermets, and Cemented Carbides
-
Published:2021
Abstract
This chapter concerns itself with the tribology of ceramics, cermets, and cemented carbides. It begins by describing the composition and friction and wear behaviors of aluminum oxide, silicon carbide, silicon nitride, and zirconia. It then compares and contrasts the microstructure, properties, and relative merits of cermets with those of cemented carbides.
Sign in
ASM members
Member Sign InTribological Properties of Ceramics, Cermets, and Cemented Carbides, Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications, By Kenneth G. Budinski, Steven T. Budinski, ASM International, 2021, p 271–300, https://doi.org/10.31399/asm.tb.tpsfwea.t59300271
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.