Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications
Chapter 4: Types of Wear and Erosion and Their Mechanisms
-
Published:2021
Abstract
This chapter covers common types of erosion, including droplet, slurry, cavitation, liquid impingement, gas flow, and solid particle erosion, and major types of wear, including abrasive, adhesive, lubricated, rolling, and impact wear. It also covers special cases such as galling, fretting, scuffing, and spalling and introduces the concepts of tribocorrosion and biotribology.
Sign in
ASM members
Member Sign InTypes of Wear and Erosion and Their Mechanisms, Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications, By Kenneth G. Budinski, Steven T. Budinski, ASM International, 2021, p 79–120, https://doi.org/10.31399/asm.tb.tpsfwea.t59300079
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.