Chapter 1: Tribology, Tribosystems, and Related Terminology
-
Published:2021
Abstract
This chapter provides information on the biennial International Wear of Materials Conference, which is the inspiration for this book. It reviews the fundamentals of tribology, tribosystems, and related terminology. The glossary at the end of this chapter is intended to familiarize readers with some of the fundamental tribology terms that will be repeated throughout this book.
Sign in
ASM members
Member Sign InTribology, Tribosystems, and Related Terminology, Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications, By Kenneth G. Budinski, Steven T. Budinski, ASM International, 2021, p 1–12, https://doi.org/10.31399/asm.tb.tpsfwea.t59300001
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.