Carburizing: Microstructures and Properties
Chapter 7: Postcarburizing Thermal Treatments
-
Published:1999
Abstract
This chapter familiarizes readers with tempering and refrigeration treatments and their effect on case-carburized parts. It explains how tempering makes such parts easier to machine, more structurally and dimensionally stable, and more durable in certain applications. It identifies key process parameters and provides test data showing how they affect hardness, yield strength, bending and contact fatigue, and fracture toughness. It also addresses potential problems stemming from process-related factors such as the presence of hydrogen and the effects of aging and grinding. In regard to refrigeration, the chapter explains that it is not uncommon for subzero treatments to be included...
Sign in
ASM members
Member Sign InPostcarburizing Thermal Treatments, Carburizing: Microstructures and Properties, By Geoffrey Parrish, ASM International, 1999, p 171–198, https://doi.org/10.31399/asm.tb.cmp.t66770171
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.